Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 12.8 g/micron | 325 g/mil | ASTM D1922 |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Elmendorf Tear Strength, MD | 12.8 g/micron | 325 g/mil | ASTM D1922 |
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |