Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 12.2 g/micron | 310 g/mil | ASTM D1922 |
ExxonMobil LD 136.MV Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Elmendorf Tear Strength, MD | 12.2 g/micron | 310 g/mil | ASTM D1922 |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Elmendorf Tear Strength, MD | 12.2 g/micron | 310 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng.. |
|||
Elmendorf Tear Strength, MD | 12.2 g/micron | 310 g/mil | ASTM D1922 |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Elmendorf Tear Strength, MD | 12.2 g/micron | 310 g/mil | ASTM D882 |
Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens,.. |