Polymer Property : Elmendorf Tear Strength, MD = 30.5 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.20 g/micron
30.5 g/mil
ASTM D1922
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
Elmendorf Tear Strength, MD 1.20 g/micron
30.5 g/mil
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..
Elmendorf Tear Strength, MD 1.20 g/micron
30.5 g/mil
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati..
Elmendorf Tear Strength, MD 1.20 - 15.7 g/micron
30.5 - 400 g/mil
Average value: 7.69 g/micron Grade Count:136
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..