Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.80 g/micron | 96.5 g/mil | |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Elmendorf Tear Strength, MD | 3.80 g/micron | 96.5 g/mil | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Elmendorf Tear Strength, MD | 3.80 g/micron | 96.5 g/mil | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Elmendorf Tear Strength, MD | 3.80 g/micron | 96.5 g/mil | |
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |
|||
Elmendorf Tear Strength, MD | 3.80 g/micron | 96.5 g/mil | ISO 6383/2 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |