Polymer Property : Elmendorf Tear Strength, MD = 239 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 9.40 g/micron
239 g/mil
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 ..