Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.82 g/micron | 224 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Elmendorf Tear Strength, MD | 8.82 g/micron | 224 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Elmendorf Tear Strength, MD | 8.80 g/micron | 224 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu.. |
|||
Elmendorf Tear Strength, MD | 8.80 g/micron | 224 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |