Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.27 g/micron | 210 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 1012CA Film Resin
(discontinued **) Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a.. |
|||
Elmendorf Tear Strength, MD | 8.27 g/micron | 210 g/mil | ASTM D1922 |
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 8.27 g/micron | 210 g/mil | ASTM D1922 |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |