Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio.. |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: slip, antiblock, and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blendedApplications: thick .. |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D1922 |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D-1922 |
Bapolene® 152A Polyethylene Film Grade Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D-1922 |
Bapolene® 152B Polyethylene Film Grade Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D-1922 |
Bapolene® 152F Polyethylene Film Grade Bapolene 152F is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Elmendorf Tear Strength, MD | 17.7 g/micron | 450 g/mil | ASTM D-1922 |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |