Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Blown Film at 1 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Blown Film at 1 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62009H Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | ASTM D1922 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Elmendorf Tear Strength, MD | 15.7 g/micron | 400 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |