Polymer Property : Elmendorf Tear Strength, MD = 15.2 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D1922
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin
Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D 1922
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D1922
Reliance Industries Relene E52009 Polyethylene
Relene E52009 is a High Density Polyethylene grade with low gel content, excellent orientation characteristics and negligible water carry-over. This grade is recommended for making raffia tapes and..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ISO 6383-2
Total PPH 4026 Polypropylene Homopolymer, Film
Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D1922
Eastman Eastobond 19411 Copolyester, Film
Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D1922
Eastman Eastobond 19412 Copolyester, Film
Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ASTM D1922
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras..
Elmendorf Tear Strength, MD 0.600 - 1.60 g/micron
15.2 - 40.6 g/mil
Average value: 0.940 g/micron Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Elmendorf Tear Strength, MD 0.600 g/micron
15.2 g/mil
ISO 6383-2
Total XSene® HD55110 High Density Polyethylene - Blown Film
HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl..
Elmendorf Tear Strength, MD 0.600 - 1.80 g/micron
15.2 - 45.7 g/mil
Average value: 1.40 g/micron Grade Count:5
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..