Polymer Property : Elmendorf Tear Strength, MD = 125 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 4.92 - 5.31 g/micron
125 - 135 g/mil
(direction not reported), Propagation Tear Strength; ASTM D-1922
Saint-Gobain Norton® PFA Fluoropolymer Film
Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti..
Elmendorf Tear Strength, MD 4.92 g/micron
125 g/mil
ASTM D1922
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed..
Elmendorf Tear Strength, MD 4.92 g/micron
125 g/mil
Blown Film at 1.25 mil; ASTM D-1922
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE
Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi..
Copyright © lookpolymers.com All Rights Reserved