Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD >= 4.72 g/micron
>= 120 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD >= 4.72 g/micron
>= 120 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil LL 1002.32 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil LL 1002x74 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil LL 1002x79 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I..
Elmendorf Tear Strength, MD >= 4.72 g/micron
>= 120 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD >= 4.72 g/micron
>= 120 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil Escorene® LD-318 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil Escorene® LD-319 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film
Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film
Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil LL 1002.09 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Elmendorf Tear Strength, MD 4.72 g/micron
120 g/mil
ASTM D1922
ExxonMobil LL 1002x75 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..