Polymer Property : Elmendorf Tear Strength, MD = 114 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 4.50 g/micron
114 g/mil
ASTM D1922
SABIC 218B Linear Low Density Polyethylene for Cast Film
Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..