Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi..
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..
Elmendorf Tear Strength, MD 11.0 g/micron
279 g/mil
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2267A Polyethylene resin is a high performance blown film polymer offering superior load retention and toughness for a variety of stretch film packaging applications. This material complies..
Elmendorf Tear Strength, MD 11.0 g/micron
280 g/mil
ASTM D1922
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design..
Elmendorf Tear Strength, MD 11.0 g/micron
279 g/mil
ASTM 1922
Braskem LH 0820/30 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Lamination; heavy duty bags; blends with LDPE and HDPE; valvulated heavy duty bags. Information provided by Braske..
Elmendorf Tear Strength, MD 11.0 g/micron
279 g/mil
ASTM D1922
ExxonMobil Exceed™ 2018EB Blown Film Resin  (discontinued **)
Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui..