Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 1.60 g/micron
40.6 g/mil
ASTM D 1922
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin
FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-..
Elmendorf Tear Strength, MD 1.60 g/micron
40.6 g/mil
Dow HDPE 05862N High Density Polyethylene
Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.