Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, MD = 0.787 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
ASTM D1922
ExxonMobil OPTEMA™ TC 115 Blown Film Resin  (discontinued **)
OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
Notched; ASTM D1922
Chevron Phillips HiD® 9640 HDPE Blown Film Resin  (discontinued **)
Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden..
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD 767.MJ Blown Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
1 mil; ASTM D1922
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer
Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide..
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
Calculated from mfr's report of 1.1 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
Calculated from mfr's report of 1.6 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 411 Paper, 7 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Elmendorf Tear Strength, MD 0.787 g/micron
20.0 g/mil
ASTM D882
Dow XU 66129.00 Developmental Monolayer Adhesive Film
XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid ure..
Elmendorf Tear Strength, MD 0.787 - 5.51 g/micron
20.0 - 140 g/mil
Average value: 4.32 g/micron Grade Count:5
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m..
Copyright © lookpolymers.com All Rights Reserved