Polymer Property : Elmendorf Tear Strength, MD = 0.591 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.591 g/micron
15.0 g/mil
ASTM D1922
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer
Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These pr..
Elmendorf Tear Strength, MD 0.591 g/micron
15.0 g/mil
Notched; ASTM D1922
Chevron Phillips HiD® 9632 HDPE Blown Film Resin  (discontinued **)
Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre..
Elmendorf Tear Strength, MD 0.591 - 0.748 g/micron
15.0 - 19.0 g/mil
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Elmendorf Tear Strength, MD 0.591 - 0.748 g/micron
15.0 - 19.0 g/mil
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..
Elmendorf Tear Strength, MD 0.591 g/micron
15.0 g/mil
ASTM D1922
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness..
Elmendorf Tear Strength, MD 0.591 g/micron
15.0 g/mil
ASTM D1922
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...