Polymer Property : Elmendorf Tear Strength, MD = 0.300 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.300 g/micron
7.62 g/mil
ASTM D1922
Lotte Chemical Titan TITANZEX® HF7000 High density polyethylene
HF7000 is a high density polyethylene resin for tubular film extrusion. HF7000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1..
Elmendorf Tear Strength, MD 0.300 g/micron
7.62 g/mil
ASTM D1922
Lotte Chemical Titan TITANZEX® HF7700 High density polyethylene
HF7700 is a high density polyethylene resin for tubular film extrusion. HF7700 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1..
Elmendorf Tear Strength, MD 0.300 g/micron
7.62 g/mil
ASTM D1922
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin
HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci..
Elmendorf Tear Strength, MD 0.300 g/micron
7.62 g/mil
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces..
Elmendorf Tear Strength, MD 0.300 - 8.30 g/micron
7.62 - 211 g/mil
Average value: 2.01 g/micron Grade Count:17
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..