Polymer Property : Film Tensile Strength at Yield, TD = 45.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ISO 527
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ISO 527
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ISO 527
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film
Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PC 1431
PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Film Tensile Strength at Yield, TD >= 45.0 MPa
>= 6530 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4252A (524H1) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ASTM D882
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used..
Film Tensile Strength at Yield, TD 45.0 MPa
6530 psi
ASTM D882
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..