Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 200 MPa | 29000 psi | Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Film Tensile Strength at Yield, TD | 200 MPa | 29000 psi | Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 250 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Film Tensile Strength at Yield, TD | 200 MPa | 29000 psi | Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 350 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Film Tensile Strength at Yield, TD | 200 MPa | 29000 psi | Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® WN, 250 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |