Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 12.4 MPa | 1800 psi | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
Film Tensile Strength at Yield, TD | 12.4 MPa | 1800 psi | 2in/min; ASTM D882 |
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform.. |
|||
Film Tensile Strength at Yield, TD | 12.4 MPa | 1800 psi | ASTM D882 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Yield, TD | 12.4 MPa | 1800 psi | ASTM D882 |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Yield, TD | 12.4 MPa | 1800 psi | ASTM D882 |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |