Polymer Property : Film Tensile Strength at Yield, TD = 11.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 11.6 MPa
1680 psi
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade
DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21..
Film Tensile Strength at Yield, TD 11.6 MPa
1680 psi
Dow LDPE 494A Low Density Polyethylene, Film Grade
DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density..