Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, TD = 10.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 136.MV Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 136.NI Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
ASTM D882
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copo..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
Blown; ASTM D822
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
Dow LDPE 586A Low Density Polyethylene, Packaging Grade
DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio..
Film Tensile Strength at Yield, TD 10.7 MPa
1550 psi
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade
DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl..