Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 10.03 MPa | 1455 psi | ASTM D882 |
Dow DOWLEX™ 2056G Linear Low Density Polyethylene Improved thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |