Mechanical Properties Metric English Comments
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Bruger, 0.2 sec; ExxonMobl Method
ExxonMobil Bicor™ 15MB440 OPP Film
Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin ..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Bruger, 0.2 sec; ExxonMobl Method
ExxonMobil Bicor™ 15MB440 OPP Film
Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin ..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Bruger, 0.2 sec; ExxonMobl Method
ExxonMobil Bicor™ 19MB440 OPP Film
Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Bruger, 0.2 sec; ExxonMobl Method
ExxonMobil Bicor™ 21MB621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
Otto Bruger, 0.2 sec, PVdC; ExxonMobl Method
ExxonMobil Bicor™ 21MB777 OPP Film
Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
510 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 26MB600 OPP Film
Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
PVdC, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 26MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
510 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Acrylic, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 26MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
510 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Brugger, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 32MB600 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As..
Seal Strength 510 g/25 mm

@Pressure 0.276 MPa,
Temperature 140 °C
510 g/in

@Pressure 40.0 psi,
Temperature 284 °F
PVdC, 0.2 sec; ExxonMobil Method
ExxonMobil Bicor™ 32MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin..