Polymer Property : Puncture Resistance = 1350 lb (f) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Resistance 6000 N

@Temperature -30.0 °C
1350 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..