Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.852 - 6.74 GPa | 124 - 978 ksi | Average value: 3.53 GPa Grade Count:15 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |