Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0621 GPa | 9.00 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.0621 GPa | 9.00 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10/F35 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |