Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 5.80 GPa
841 ksi
Calculated
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC
Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st..
Shear Modulus 5.80 GPa
841 ksi
Calculated
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Shear Modulus 5.80 GPa
841 ksi
Calculated
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Shear Modulus 5.80 GPa
841 ksi
Calculated
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..