Polymer Property : Shear Modulus = 4.726 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.726 GPa
685.5 ksi
ASTM C273
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
Shear Modulus 4.726 GPa
685.5 ksi
ASTM C273
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI
LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow.