Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0296 GPa | 4.30 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0296 GPa | 4.30 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10/F35 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |