Mechanical Properties Metric English Comments
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 1205 Glass Reinforced SMC
Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2205-20 CRSX Polyester SMC
Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Premix Premi-Glas® 3404 33% Glass Reinforced SMC
Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required...
Shear Modulus 3.80 GPa
551 ksi
Calculated
Plenco 7466 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406..
Shear Modulus 3.80 GPa
551 ksi
in plane
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP
SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f..
Shear Modulus 3.80 GPa
551 ksi
in plane
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP
SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit
Shear Modulus 3.80 GPa
551 ksi
in plane
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP
SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc..
Shear Modulus 3.80 GPa
551 ksi
Calculated
Plenco 4466 Phenolic, Granular, Transfer Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Shear Modulus 3.80 GPa
551 ksi
calculated
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
Copyright © lookpolymers.com All Rights Reserved