Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 24.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 24.0 GPa
3480 ksi
calculated
Piezo Kinetics 532 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type V, this ceramic is used as sensors that require low impedance, high dielectric constant and high sensitivity.Elastic Compliance s11E (x 10-12 m²/n): 15.9.Elastic Compliance s33..
Shear Modulus 24.0 GPa
3480 ksi
calculated
Piezo Kinetics 556 Lead Zirconate Titanate Piezoelectric
Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val..
Shear Modulus 24.0 GPa
3480 ksi
calculated
Schott F5 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 24.0 GPa
3480 ksi
calculated
Schott LF5 Glass
Information Provided by SCHOTT North America, Inc.
Copyright © lookpolymers.com All Rights Reserved