Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.0200 GPa | >= 2.90 ksi | ASTM C273 |
Parabeam Industrie ParaTank 6 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Modulus | 0.0200 GPa | 2.90 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | >= 0.0200 GPa | >= 2.90 ksi | ASTM C393 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Shear Modulus | >= 0.0200 GPa | >= 2.90 ksi | ASTM C393 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Shear Modulus | 0.0200 GPa | 2.90 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |