Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.700 GPa | 102 ksi | DIN 53457 |
Global PP-1102-K Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-textile applications, bags, tape, sheetInformation provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.700 GPa | 102 ksi | DIN 53457 |
Global PP-1126-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.700 GPa | 102 ksi | ISO 6721-2 |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Shear Modulus | 0.703 GPa | 102 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/8-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.703 GPa | 102 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.700 GPa | 102 ksi | torsional |
DSM Fibre Intermediates Nyrim® 2000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Shear Modulus | 0.700 GPa | 102 ksi | calculated |
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
(discontinued **) Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5.. |
|||
Shear Modulus | 0.704 GPa | 102 ksi | Calculated |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |