Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.750 - 1.45 GPa | 109 - 210 ksi | Average value: 1.27 GPa Grade Count:9 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Shear Modulus | 0.750 GPa | 109 ksi | Calculated |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Shear Modulus | 0.750 GPa | 109 ksi | ISO 6721-2 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Shear Modulus | 0.750 - 0.930 GPa | 109 - 135 ksi | calculated |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |