Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.121 GPa @Temperature -50.0 - 150 °C |
>= 17.5 ksi @Temperature -58.0 - 302 °F |
Average value: 0.724 GPa Grade Count:11 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Shear Modulus | 0.121 GPa | 17.5 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 9.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.121 - 0.345 GPa | 17.5 - 50.0 ksi | |
ERG Aerospace Duocel® Aluminum Metal Foam |