Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0345 GPa | 5.00 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 1/4 - 3.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.0345 GPa | 5.00 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.0345 GPa | 5.00 ksi | Plate Shear, W Direction, typ, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |