Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.95 GPa @Temperature 23.0 °C |
1440 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15330 NC010 PBT
(Unverified Data**) Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Modulus | 9.95 GPa | 1440 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® CE15330 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 NC010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V.. |