Polymer Property : Tensile Modulus = 9.90 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527-1/-2
DSM Arnite® CCT GF30 (T-X01301) PBT-30% Glass Reinforced (European Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Tensile Modulus 9.90 GPa
1440 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Tensile Modulus 9.90 GPa
1440 ksi
Radici Radilon® S RV300R (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527-1,-2
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527-1,-2
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Modulus 9.90 GPa
1440 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
Tensile Modulus 9.90 GPa
1440 ksi
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned
Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is ..
Tensile Modulus 9.90 GPa
1440 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6
LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant.
Tensile Modulus 9.90 GPa
1440 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 (Asia Pacific)
LNP* Lubricomp* PFL-4216 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66
LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66
LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East)
Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East)
LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive.
Tensile Modulus 9.90 GPa
1440 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Tensile Modulus 9.90 GPa
1440 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Tensile Modulus 9.90 GPa
1440 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Tensile Modulus 9.90 GPa
1440 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon
LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527
Polyram RamSter PF306G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram.
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Plenco 4300 Phenolic, Granular, Injection Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Plenco 4304 Phenolic, Nodular, Injection Molded
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component ..
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Plenco 4504 Phenolic, Granular, Injection Molded
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c..
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527-1/-2
DSM Arnite® TV4 461 (PBT+PET)-GF30
30% Glass Reinforced
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527-1/-2
DSM Arnite® TV4 461 KL (PBT+PET)-GF30
30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties
Tensile Modulus 9.90 GPa
1440 ksi
1mm/min; ISO 527
BASF Ultradur S 4090 G6 LS High Speed BK15077 30% Glass Filled PBT
Ultradur S 4090 G6 LS High Speed BK15077 is a high flow, fast cycling with low warpage, 30% glass filled injection molding PBT.
Tensile Modulus 9.90 GPa
1440 ksi
ISO 527-1/-2
DSM Arnite® TV4 261 KL PBT-GF30
30% Glass Reinforced, Light Stabilized
Tensile Modulus 9.90 GPa
1440 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret..
Tensile Modulus 9.90 GPa
1440 ksi
Radici Radilon® A RV350 (cond) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Plenco 1506 Polyester, Briquette, Injection Molded
PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop..
Tensile Modulus 9.90 GPa
1440 ksi
1mm/min; ISO 527
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry)
Ultramid N-265 NF3001 is a general purpose, 40% mineral reinforced PA6/6 that provides excellent flatness and dimensional stability in injection molding.
Copyright © lookpolymers.com All Rights Reserved