Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.29 GPa | 1350 ksi | ASTM D638 |
Plenco 51335 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51335 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in black only.Information .. |