Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.21 GPa | 1340 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 9.21 GPa @Temperature -40.0 °C |
1340 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |