Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.15 GPa | 1330 ksi | |
Radici Radilon® S RV300LK (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 9.15 GPa | 1330 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |