Polymer Property : Tensile Modulus = 879 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.06 GPa
879 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Modulus 6.06 GPa
879 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66
LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 6.06 GPa
879 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
Tensile Modulus 6.06 GPa
879 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66
LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant.
Tensile Modulus 6.06 GPa
879 ksi
1mm/min; ISO 527
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
Ultramid B3EG3 BK00564 is a 15% glass fiber reinforced, pigmented black injection molding PA6 grade for housings with enhanced impact resistance.