Mechanical Properties Metric English Comments
Tensile Modulus 5.93 GPa

@Temperature 150 °C
860 ksi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Tensile Modulus 5.93 GPa

@Temperature 150 °C
860 ksi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Tensile Modulus 5.93 GPa
860 ksi
ASTM D638
Westlake Plastics Zelux® 20% GF Polycarbonate 20% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Tensile Modulus 5.93 GPa
860 ksi
ASTM D638
Ensinger Tecanat™ GF20 20% Glass Reinforced Polycarbonate (PC)
Tenacat™ GF20 is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for ..
Tensile Modulus 5.93 GPa
860 ksi
ASTM D638
Quantum Polycarbonate 20% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
Tensile Modulus 5.93 GPa
860 ksi
ASTM D638
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding
20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.
Tensile Modulus 5.93 GPa
860 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS
LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend.