Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 822 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 5.67 GPa
822 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific)
LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Tensile Modulus 5.67 GPa
822 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
Copyright © lookpolymers.com All Rights Reserved