Polymer Property : Tensile Modulus = 80.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works.
Tensile Modulus 0.276 - 0.552 GPa
40.0 - 80.0 ksi
Master Bond LED401 One Component LED Curable Adhesive System
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In..
Tensile Modulus 0.276 - 0.552 GPa
40.0 - 80.0 ksi
Master Bond LED403Med USP Class VI, One Component, LED Curable System
Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi..