Polymer Property : Tensile Modulus = 8.72 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.72 GPa
1260 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC
LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare.
Tensile Modulus 8.72 GPa
1260 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU
LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.