Polymer Property : Tensile Modulus = 8.48 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.48 GPa
1230 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Modulus 8.48 GPa
1230 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Modulus 8.48 GPa
1230 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Clean Compounding System, Electrically Conductive, Wear Resistant, Ea..
Tensile Modulus 8.48 GPa
1230 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DEL33EC PC (Asia Pacific)
LNP STAT-KON* DEL33EC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features of this material include: Clean Compounding System.
Tensile Modulus 8.48 GPa
1230 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10
LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 8.48 GPa
1230 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 8.48 GPa
1230 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon DX96690 PC
LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America..
Tensile Modulus 8.48 GPa
1230 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific)
LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 8.48 GPa
1230 ksi
ASTM D638
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement  (discontinued **)
Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ..
Tensile Modulus 8.48 GPa
1230 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10
LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.