Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.34 GPa | 1210 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Tensile Modulus | 8.34 GPa | 1210 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |